| Core loss | Boron Nitride multiwall nanotube | BN | N K | 370.5 – 747.9 eV | 100 kV | 0.7 eV | Odile Stephan | 2008-02-07 |
| Low loss | Boron Nitride single wall nanotube | BN | | 4 – 30.7 eV | 100 kV | 0.2 eV | Odile Stephan | 2008-02-25 |
| Low loss | Boron Nitride triple wall nanotube | BN | | 4 – 30 eV | 100 kV | 0.2 eV | Odile Stephan | 2008-02-25 |
| Core loss | h-BN CVD | BN | | 180 – 250.1 eV | 60 kV | 0.06 eV | Andrey Chuvilin | 2021-05-22 |
| Low loss | Hexagonal Boron Nitride | BN (hex) | | -61.5 – 450 eV | 300 kV | 1.2 eV | Giovanni Bertoni | 2007-11-12 |
| Core loss | Hexagonal Boron Nitride | BN (hex) | B K, N K | 113.5 – 625 eV | 300 kV | 1.2 eV | Giovanni Bertoni | 2007-11-12 |
| Core loss | Reduced graphene oxide | C | C K | 244.5 – 551.4 eV | 300 kV | | Edgar Jimenez | 2014-01-29 |
| Core loss | Diamond | C | C K | 265.6 – 367.5 eV | 100 kV | 1.8 eV | Virginie Serin | 2005-04-20 |
| Low loss | Diamond | C | | -11.4 – 90.5 eV | 100 kV | 1.8 eV | Virginie Serin | 2005-04-20 |
| Low loss | Diamond | C | | -6.1 – 44.9 eV | 100 kV | 1.6 eV | Virginie Serin | 2005-04-20 |
| Core loss | Graphite | C | C K | 268.3 – 370.2 eV | 100 kV | 1.2 eV | Virginie Serin | 2005-04-20 |
| Low loss | Graphite | C | | -10.7 – 91.2 eV | 100 kV | 1.2 eV | Virginie Serin | 2005-04-20 |
| Low loss | diamond | C | | 283.7 – 305 eV | 60 kV | 0.19 eV | Virginie Serin | 2005-04-20 |
| X-ray absorption | Diamond | C | C K | 277.8 – 379.7 eV | 800 kV | | Michel Jaouen | 2005-04-20 |
| X-ray absorption | Diamond | C | C K | 260 – 600 eV | 800 kV | 0.2 eV | Michel Jaouen | 2005-04-20 |
| Low loss | Carbon double wall nanotube | C | | -5.9 – 45.3 eV | 100 kV | 0.7 eV | Odile Stephan | 2008-02-25 |
| Low loss | Carbon multi wall nanotube | C | | -1.4 – 49.8 eV | 100 kV | 0.7 eV | Odile Stephan | 2008-02-25 |
| Low loss | Carbon single wall nanotube | C | | -2.5 – 48.6 eV | 100 kV | 0.7 eV | Odile Stephan | 2008-02-25 |
| Core loss | Carbon single wall nanotube | C | C K | 260.1 – 360.9 eV | 80 kV | 0.5 eV | Odile Stephan | 2008-02-25 |
| Low loss | Amorphous Carbon | C (amorphous) | | -8.3 – 44.5 eV | 200 kV | 1 eV | Dr. Graham Carpenter | 2009-05-13 |
| Core loss | Graphite (really glassy carbon) | C (graphite) | C K | 269.8 – 313.9 eV | 100 kV | 0.5 eV | David Muller | 2005-04-20 |
| Core loss | Cubic boron nitride | c-BN | B K | 167.7 – 262.2 eV | 400 kV | 1.8 eV | Dr. Gilles Hug | 2005-04-20 |
| Core loss | Cubic boron nitride | c-BN | N K | 381.1 – 462.2 eV | 400 kV | 1.8 eV | Dr. Gilles Hug | 2005-04-20 |
| Core loss | Oxidized-graphenic nanoplatelets obtained from bamboo - high oxygen | C-O | C K | 241.8 – 344.6 eV | 80 kV | 0.6 eV | Luc Lajaunie | 2016-08-24 |
| Core loss | Oxidized-graphenic Nanoplatelets Obtained From Bamboo - high oxygen | C-O | C K, O K | 211.7 – 623.2 eV | 80 kV | 0.8 eV | Luc Lajaunie | 2016-08-24 |
| Core loss | Oxidized-graphenic Nanoplatelets Obtained From Bamboo – Low Oxygen | C-O | C K | 241.6 – 344.1 eV | 80 kV | 0.6 eV | Luc Lajaunie | 2016-08-24 |
| Core loss | Oxidized-graphenic Nanoplatelets Obtained From Bamboo – Low Oxygen | C-O | C K, O K | 201.3 – 616.8 eV | 80 kV | 0.8 eV | Luc Lajaunie | 2016-08-24 |
| Core loss | Melamine Powder | C3N6H6 | C K | 257.1 – 467.6 eV | 100 kV | | Susana Trasobares | 2007-11-19 |
| Core loss | Melamine Powder -Irradiated | C3N6H6 | C K | 244.4 – 457.2 eV | 100 kV | | Susana Trasobares | 2007-11-19 |
| Core loss | CaCoO Misfit Nanotube | CaCoO2−CoO2 | Ca L1, Ca L2,3, Co L2,3, O K | 254.8 – 1099.6 eV | 200 kV | 1.5 eV | Luc Lajaunie | 2016-06-12 |
| Low loss | Calcium titanate (perovskite structure) | CaTiO3 | | -20 – 184.2 eV | 200 kV | 1 eV | Saso Sturm | 2007-12-05 |
| Core loss | Calcium titanate (perovskite structure) | CaTiO3 | Ca L2,3 | 260 – 438.6 eV | 200 kV | 1 eV | Saso Sturm | 2007-12-05 |
| Core loss | Calcium titanate (perovskite structure) | CaTiO3 | O K, Ti L2,3 | 400 – 604.2 eV | 200 kV | 1 eV | Saso Sturm | 2007-12-05 |
| Low loss | Calcium Titanate (polycrystalline layer) | CaTiO3 | Ti M2,3 | 0.1 – 61.5 eV | 80 kV | 0.18 eV | Andreas Krause | 2016-05-10 |
| Low loss | Calcium Titanate (polycrystalline layer) | CaTiO3 | | 0.2 – 20.7 eV | 80 kV | 0.18 eV | Andreas Krause | 2016-05-10 |
| Core loss | Cerium Praseodymium mixed oxide | CePrOx | Ce M4,5, Pr M4,5 | 853.2 – 1057.8 eV | 200 kV | | Susana Trasobares | 2007-11-19 |
| Core loss | Cerium Praseodymium mixed oxide supported on Al2O3 doped with La2O3 | CePrOx/Al2O3-La2O3 | Ce M4,5, La M4,5, Pr M4,5 | 758.1 – 1065 eV | 200 kV | | Susana Trasobares | 2007-11-19 |
| Core loss | CN crystal | CN | C K | 262.4 – 470.3 eV | 100 kV | 0.7 eV | Susana Trasobares | 2007-11-19 |
| Core loss | Metallic Cobalt | Co | Co L2,3 | 414.5 – 926 eV | 200 kV | | Yuan Zhao | 2014-07-20 |
| Core loss | cobalt | Co | Co L2,3 | 769.7 – 816.4 eV | 100 kV | 0.6 eV | Dominique Imhoff | 2008-03-04 |
| Low loss | Porous cobalt coating with He-filled nanopores | Co + He | He K | | 300 kV | 1 eV | Bertrand Lacroix | 2018-04-06 |
| Low loss | Porous cobalt coating with He-filled nanopores | Co + He | | | 300 kV | 1 eV | Bertrand Lacroix | 2018-04-06 |
| Core loss | Cobalt(II,III) oxide | Co3O4 | Co L2,3 | 412.5 – 924 eV | 200 kV | | Yuan Zhao | 2014-07-20 |
| Low loss | Cobalt (III) Oxide (IV) | Co3O4 | | -17.5 – 33.6 eV | 200 kV | 0.35 eV | xu qiang | 2007-12-11 |
| Core loss | Cobalt (III) Oxide (IV) | Co3O4 | Co L2,3 | 767 – 818.1 eV | 200 kV | 0.35 eV | xu qiang | 2007-12-11 |
| Core loss | Cobalt monoxide | CoO | Co L2,3 | 406.5 – 918 eV | 200 kV | | Yuan Zhao | 2014-07-20 |
| Low loss | Cobalt Oxide | CoO | | -17.5 – 33.6 eV | 200 kV | 0.3 eV | xu qiang | 2007-12-11 |
| Core loss | Cobalt Oxide | CoO | Co L2,3 | 767 – 818.1 eV | 200 kV | 0.3 eV | xu qiang | 2007-12-11 |
| Core loss | cobalt oxide | CoO | O K | 518 – 605.3 eV | 100 kV | 0.6 eV | Dominique Imhoff | 2008-03-04 |
| Core loss | cobalt oxide | CoO | Co L2,3 | 748.4 – 888.4 eV | 100 kV | 0.6 eV | Dominique Imhoff | 2008-03-04 |