background removed
calibration : 1- XAS energy reference from standard similar LSMO (maximum of MnL3 peak)
2- energy dispersion calibration of the detector from two peaks reference in low and core loss areas (STO substrate area in the multimayer system).
see also LaM,OK Analyst: imhoff. Temperature: Room.
Use in HyperSpy
import exspy
spectra = exspy.data.eelsdb(title="LSMO perovskite", formula="(La0.7,Sr0.3)MnO3")
s = next(sp for sp in spectra if sp.original_metadata.json.id == 21737)
s.plot(plot_edges=True)
Specimen
Formula
(La0.7,Sr0.3)MnO3
Elements
La, Sr, Mn, O
Edges
Mn L2,3
Source and purity
perovskite multilayers UMP CNRS-Thales Palaiseau France (laser ablation)
Energy range
633.29 – 662.4 eV
Step
0.229 eV
Keywords
imported from old site
Treatment
Dark current corrected
Yes
Gain variation corrected
No
Acquisition
Microscope
STEM-VG
Gun
Cold FEG
Beam energy
100 kV
Convergence semi-angle
7 mrad
Collection semi-angle
22 mrad
Mode
STEM
Detector
Parallel: 666 + CCD modified Orsay
Probe size
0.7 nm²
Integration time
0.2 s
Readouts
10
Reference
EELS study of interfaces in magnetoresistive LSMO/STO/LSMO tunnel junctions
Samet L., Imhoff D., Maurice J-L., Contour J-P., Gloter A., Manoubi T., Fert A., Colliex C.,